CHONBURI
According to the mixing ratio, our workers will get the raw powder, clay, and additives fully and evenly mixed in a mixer, preparing for the stage of ball making or kneading and extrusion.
We will add the mixed materials, additives and water to the kneader to obtain a highly uniform and relatively humid material. It can ensure the compressive strength and density of our products.
The mixture is nucleated in a ball forming machine to reach a certain particle size, and then sieved and hardened to obtain an intermediate product with strength and a smooth and hard surface.
Remove the moisture and organic additives contained in the molecular sieve intermediate product while maintaining the precursor of the molecular sieve intact to obtain a shaped molecular sieve product with excellent performance.
Our workers will put the qualified product into a sealed Ace box first, and then puts it into sealed barrels or other packaging like bags and cartons after it cools down to avoid exposure to the air.
Though, there are property tests conducted at every production stage, we will take samples from each batch of product to do representative tests and make a comprehensive analysis to ensure its performance.
Contact Us
JALON MICRO NANO NEW MATERIALS CO. LTD
NO. 890/68 Moo 3, KHAO KHANSONG, SI RACHA, CHONBURI - 20110, Thailand
Mobile : +66-971585837224
E-mail : himanshu.sharma@jalonzeolite.com
Hi! Simply click below and type your query.
Our experts will reply you very soon.